Solutions

Barrier Films


Typical Thickness: 2.0 – 6.0 mils (50 – 150 microns) 
Output: 450 - 600 lbs./hr.

Typical Line Configuration

Extruder Package: 

Two 2.5" (65mm) 30:1 & Five 2.0" (50 mm) 30:1 for 7 Layers

Nine 2.0" (50mm) 30:1 for 9 Layers

Screen Changer: 

 

Die Package:

16" - 18" Typically

Air Ring:

Dual lip technology

IBC: 

Digisonic Internal Bubble Cooling

Bubble Cage: 

Segmented Rollers or air cage

Collapsing Frames:

Covered slats

Primary Nip: 

Typical width 74" (1880 mm)

Thickness Gauge: 

Yes

Secondary Nip:

 Yes

Treater: 

Optional

Winder:

GEC 1008

Controls:  

GEC Process Control

Gravimetrics/Blending/Scrap Reclaim:

Material Handling Systems

Additional Equipment: